Tracy,
I'm the (one of the?) guys that use compressed air in with the plates. I couldn't tell you why, cause most don't. But RJ and friends never said it would hurt. One interesting thing that happens to me is I don't get much of a hardness increase with cryo and S30V. (snap temper or not) I asked about that before and was told not to worry about it; it just means my quench process is working well for me, but to keep up the cryo. Steve |
#32
|
||||
|
||||
Thanks Quench.I apprecaite it.
Sorry Steve, I just recall who was doing that. I think it makes perfect sense. I need to try that, I just haven't wheeled my compressor over from one garage to the other yet but I will the next blade I do and report back on the results. |
Tags |
blade, forge, knife, knives |
Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
Thread Tools | |
Display Modes | |
|
|