Carpenter XHP
Hello gents! I've got my first four blades of Carpenter's XHP ready to HT. I have the Carpenter recomendations at hand - 1900, 550 1 hour - but I was figuring that somebody has already done a little experimentation that I might could "borrow" from their experience
My blades are all 1/8 thick, I was planning on foil treating them and plate quenching. I was also going to cryo them post quench like 40CP but should I wait post temper??? The spec sheet says you can push the hardness to 64ish with a 350 temper but that seems like it might get a little brittle....or would it? Dang sure may be hard to sharpen __________________ Dennis "..good judgement comes from experience, experience comes from poor judgement.." -Gary McMahan, a cowboy poet and good dancer. http://www.facebook.com/home.php#!/p...24112090995576 |
Tags |
post |
Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
|
|
Similar Threads | ||||
Thread | Thread Starter | Forum | Replies | Last Post |
Carpenter O1 | HellForged | The Supply Center | 3 | 11-05-2004 11:44 AM |
Has anyone tried 440-XH or CRB-7 from Carpenter Tech. | T L Smith | High-Performance Blades | 10 | 02-17-2004 07:40 AM |