Okay, a little bit of closure.
Went back to the machine shop for some more hardness testing. The machine is working properly now. Test results: HRC 60 calibration sample: tests at 60 as-quenched test coupon tests at 61.5, a little low, but I'll take it tempered coupon tests at 60 knife (mid tang) tests at 60.5 So, my numbers are a little low, could be that I didn't cool quickly enough in quench, moving the blade fore and aft in the bath may improve the outcome on future blades. I also suspect that thinner sections, closer to the cutting edge cooled faster than the thick section of the tang, resulting in slightly higher values, but I didn't want to mar a visible portion of the blade. Thanks again for all the help, I'll post pictures once the knife is complete. -Radar |
Tags |
550, angle, blade, digital, edge, firebrick, flat, grinder, hand, heat, heat treat, hot, knife, made, material, newbie, pins, polish, post, scale, scratch, skinner, stabilizing, surface, tiny |
Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
Thread Tools | |
Display Modes | |
|
|
Similar Threads | ||||
Thread | Thread Starter | Forum | Replies | Last Post |
Re-Heat Treat? | mrgantz | Heat Treating and Metallurgy | 4 | 02-12-2010 03:42 AM |
heat treat ti | dcfolders | The Folding Knife (& Switchblade) Forum | 6 | 12-19-2009 12:01 PM |
Heat treat? | ranger1 | Heat Treating and Metallurgy | 6 | 01-21-2007 09:54 AM |
Heat treat set up. | Ray Cover Jr | The Newbies Arena | 5 | 04-16-2004 04:14 AM |
heat treat help, | Eichler | The Newbies Arena | 10 | 04-10-2004 09:48 PM |