sawblade. How to work and ht?
Hi guys
I just got a hold of this beauty: Its 0,12" thick and 25" in diameter. There are no marking on the blade and its possible to file it down. How should i go about using this steel? Should i anneal if first before working it? Should i HT as "normal" 3 normalization cycles and then try to see which hardness I get when quenchin around nonmagnetic? Last edited by Rasmus Kristens; 08-04-2019 at 11:53 AM. |
Tags |
a, blade, blades, build, ca, carbon, diy, file, files, flat, forge, forged, grinding, how to, knife, knife s, made, make, marking, motor, post, quenched, steel, tool, tool steel |
Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
|
|
Similar Threads | ||||
Thread | Thread Starter | Forum | Replies | Last Post |
New hot work | Fox Creek | The Outpost | 9 | 11-12-2007 11:33 AM |
hello all and some of my work | eklund | The Display Case | 4 | 10-04-2007 12:45 PM |
metal work sheath work available | SVanderkolff | Knife Making Discussions | 0 | 02-15-2004 08:01 PM |
Will This Work????? | DiamondG Knives | Ed Caffrey's Workshop | 1 | 07-25-2003 06:45 AM |
sawblade | birdog4 | Ed Caffrey's Workshop | 3 | 11-14-2001 07:14 AM |