Fit & Finish Fit and Finish = the difference in "good art" and "fine art." Join in, as we discuss the fine art of finish and embellishment. |
|
Thread Tools | Display Modes |
#1
|
|||
|
|||
Etching Mokume
I did use some mokume long ago when I didn't have the power of the forums for information. I believe I used some diluted muriatic acid (HCL) I do have on hand some Etchant and ferric chloride which I believe are much the same. I would certainly appreciate suggestions on what has worked well for others on the amount to mix with water and what sort of time it will take to get a good etch. Thanks Frank