I ground the samples flush with the steel. By evaluating the glue lines I've found:

1. Loctite Xtreme:

It's a thick gel like stuff. Hard to get smooth coverage. It needs a good squeeze. But the glue line looks fine.

2. Loctite U-05FL Flexible Commercial Adhesive

This stuff is a urathane (sp?) adhesive and bubbles/expands while it cures. I've used it before and learned it requires heavy clamping to keep the glueline looking good. With light clamping the glue line doesn't look so hot.


3. DEVCON 2 Ton Epoxy

Glue line is fine, but under microscope there some tiny gaps on one side - and I mean tiny. Maybe I didn't apply it perfectly right there at the edge.

4. Loctite E-120HP

Looks fine.

5. JB WELD

Leaves a thicker glue line and is visible on one side. It's thinner than I thought it would be, but will probably always show something if used for handle slabs. It's visibly not the color of stainless steel.

6. Acraglas Gel

Looks fine.

7. West Systems Epoxy (10 min Pot life)

Looks fine.

Steve