I did use some mokume long ago when I didn't have the power of the forums for information. I believe I used some diluted muriatic acid (HCL) I do have on hand some Etchant and ferric chloride which I believe are much the same. I would certainly appreciate suggestions on what has worked well for others on the amount to mix with water and what sort of time it will take to get a good etch. Thanks Frank