    Ok, I start with a light coat of viniger. applied with a 0000 steel wool pad. Then put on a coat of Ferric chloride with a small brush. While the FC is still wet I scrubb the blade with a 0000 steel wool pad dipped in viniger. I just keep repeating the process until I get the desired finish. Clean well with windex to stop the acid Then polish with a metal polish . Steel type will have alot to do with the hamon. Best results are with fast quenching steels ie 1095 and W2. O1 and such is very hard to get a line on. Hope this helps.
  2. Panvelky
    03-08-2010 09:09 AM
    Panvelky
    Hey Andy, Tell me again how you etched that blade at the last meeting. I have a blade that I did a differential quench and I want to bring that out with the acid but I could not remember how you did it and I didn't want to just stick it in. Thanks.

About Me

  • About ranger1
    Biography
    Member of the N.C.knifemakers Guild.
    Location
    Lexington,NC
  • Signature
    Andy Sharpe
    I ruin perfectly good steel!!
    www.sharpeknives.com

Statistics

Total Posts
Albums
Visitor Messages
General Information
  • Last Activity: 07-28-2018 07:39 PM
  • Join Date: 12-18-2005

Friends

Showing Friends 1 to 3 of 3

All times are GMT -5. The time now is 03:35 PM.




KNIFENETWORK.COM
Copyright © 2000
? CKK Industries, Inc. ? All Rights Reserved
Powered by ...

Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
The Knife Network : All Rights Reserved